| Material | Sintered Neodymium Iron Boron | |
| Dimensions | Diameter | Min.1 mm—Max.60 mm |
| Tolerance | Standard +/-0.05mm, Min.+/-0.02mm | |
| Magnetization Orientation | Axial / Diametrical | |
| Magnetic Properties | Grade | Max. Operating Temperatures |
| N35-N52 | 80°C (176°F) | |
| 33M- 48M | 100°C (212°F) | |
| 33H-48H | 120°C (248°F) | |
| 30SH-45SH | 150°C (302°F) | |
| 30UH-40UH | 180°C (356°F) | |
| 28EH-38EH | 200°C (392°F) | |
| 28AH-35AH | 230°C (428°F) | |
| Remanence(Br) | 11,300 Gauss — 14,800 Gauss | |
| Coercive Force(Hcb) | 10,000 Oersted — 12,600 Oersted | |
| Intrinsic Coercive Force(Hcb) | 11,000 Oersted — 36,000 Oersted | |
| Magnetic Energy Product (BH) | 33M GOe — 53M GOe | |
| Surface Treatment | Ni-Cu-Ni, Nickel, Zn, Gold, Silver, Copper, Epoxy, Chemical, PTFE, Parylene, Everlube, Passivation and more. | |